WebMar 22, 2013 · We have started having problems with craters in the paint film on the motorcycle parts we manufacture. This problem is very peculiar because it seems to come and go. For example, when we start up the line at 8 a.m. the paint film is OK, but by 9 a.m. the crater problem suddenly begins occurring. WebHOW TO FIX CRATERING IN CAR PAINT Causes for the appearance of cratering. The main causes of the appearance of cratering have to do with the presence of... Measures to …
Automotive Coatings: Application Defects
WebA. The most probable cause for the paint craters is surface tension; therefore, in my opinion I would try to change the surface tension of the oil so that it allows the paint to properly … WebHow do you fix paint craters? To solve the appearance of cratering in the paint, you must first allow the finish to dry completely, in order to correctly assess the severity of the problem. If the craters are not very large, a good solution would be to sand the surface of the part with P1500 sandpaper, and subsequently polish and glaze the surface. camp humphreys area 1
Cratering – Advice on paint defects Glasurit
WebJun 16, 2024 · Paint film defects can appear during or immediately after application or become more apparent after the coating is ... the difference in surface tension at the paint … Web#autopaintreactions #fixingpaint #carpainting Get a FREE A-Z 85 PG. Auto Body Guide Here: http://www.learnautobodyandpaint.com/free-autobody-manual/Learn how... WebMar 22, 2013 · We have started having problems with craters in the paint film on the motorcycle parts we manufacture. This problem is very peculiar because it seems to … camp humphreys apo